I have some lengths of cooper bar - 1 inc x 1/2 inch x 5 inch - used
as interconnectors on 2v battery cells. I wish to tin them and can
either cart them off to an electroplater or tin with solder. Solder
wire worked fine on a test piece with a blow torch. My question is
which solder bar to go for - lead free or leaded?? My instinct is
leadfree - tin with some silver and possible copper - something like
Sn96/Ag4.

TVMIA
 
Thread Tools Search this Thread
Search this Thread:

Advanced Search
Display Modes

Posting Rules

Smilies are On
[IMG] code is Off
HTML code is Off
Trackbacks are On
Pingbacks are On
Refbacks are On


Similar Threads
Thread Thread Starter Forum Replies Last Post
Copper bottom Terry K Boat Building 2 January 28th 08 06:37 PM
Copper tubing and sea water ian Boat Building 15 July 31st 07 09:22 PM
Copper ring report Roger Long Cruising 18 July 26th 06 01:17 AM
Copper Tubing in Propane System none Cruising 11 June 4th 04 01:43 AM
Source for Copper Bus Bar Charlie J Electronics 8 November 12th 03 12:07 AM


All times are GMT +1. The time now is 01:37 AM.

Powered by vBulletin® Copyright ©2000 - 2024, Jelsoft Enterprises Ltd.
Copyright ©2004-2024 BoatBanter.com.
The comments are property of their posters.
 

About Us

"It's about Boats"

 

Copyright © 2017