Some of y'all seem to be forgetting that a major contributing factor is the paint under the snaps.
The natural aluminum does a better job resisting.
  #42   Report Post  
posted to rec.boats
external usenet poster
 
First recorded activity by BoatBanter: Mar 2014
Posts: 811
Default Galvanic corrosion

On 5/19/2014 9:31 PM, True North wrote:
Some of y'all seem to be forgetting that a major contributing factor is the paint under the snaps.
The natural aluminum does a better job resisting.

It's the paint's fault? Come on Don get grip.
  #43   Report Post  
posted to rec.boats
Banned
 
First recorded activity by BoatBanter: Jun 2013
Posts: 1,692
Default Galvanic corrosion

On Monday, May 19, 2014 9:53:14 PM UTC-4, H*a*r*r*o*l*d wrote:

It's the paint's fault? Come on Don get grip.


Well, he IS ****ing STUPID.
  #44   Report Post  
posted to rec.boats
external usenet poster
 
First recorded activity by BoatBanter: Jul 2006
Posts: 10,492
Default Galvanic corrosion

On Mon, 19 May 2014 18:31:11 -0700 (PDT), True North
wrote:

Some of y'all seem to be forgetting that a major contributing factor is the paint under the snaps.


===

That is very unlikely. The paint blisters are a symptom not a cause.
Corrosion forms a white powder at the junction of the dissimilar
metals (Aluminum and SS), and that causes the paint to lift.
  #45   Report Post  
posted to rec.boats
Tim Tim is offline
external usenet poster
 
First recorded activity by BoatBanter: Nov 2006
Posts: 19,107
Default Galvanic corrosion

On Saturday, May 17, 2014 3:33:32 AM UTC-7, True North wrote:
Yesterday I was on the Legend website where they have a chat function.

I asked the rep about the snaps and she confirmed that they were indeed stainless steel.

She then asked if I had any other concerns.

I felt chatty so I informed her about the corrosion problem... not really expecting to much back.

She went right to the warranty manager and quoted him as saying salt water corrosion was an unpredictable process and not really a warranty problem. He also stated they didn't recommend their boats be used in salt water.

First I heard of this and no where have I seen this in writing nor did the dealer mention it.

They did say to forward pictures of the blisters and they would consult with the dealer on what to do.

Looks like I may be looking for a good Jewish lawyer.


nice for them to tell that to you now, Don. When they sold you the boat, did they ask you 'where' you'd be boating. If the did and you told them, they should have made other hull structure recomendations


  #46   Report Post  
posted to rec.boats
external usenet poster
 
First recorded activity by BoatBanter: Jan 2011
Posts: 5,756
Default Galvanic corrosion

Yes Tim, I did tell them my favorite boating destinations...which are all salt water.
Unless you have cottage on a lake and plan to just leave the boat there, you'd really be limiting yourself in this area.
All the interesting areas to cruise are on the ocean.
  #47   Report Post  
posted to rec.boats
external usenet poster
 
First recorded activity by BoatBanter: Mar 2014
Posts: 811
Default Galvanic corrosion

On 5/20/2014 6:57 AM, True North wrote:
Yes Tim, I did tell them my favorite boating destinations...which are all salt water.
Unless you have cottage on a lake and plan to just leave the boat there, you'd really be limiting yourself in this area.
All the interesting areas to cruise are on the ocean.

Does your boat builder have a dealership at an ocean location?
  #48   Report Post  
posted to rec.boats
external usenet poster
 
First recorded activity by BoatBanter: Jan 2011
Posts: 5,756
Default Galvanic corrosion

Duh, Jimmy.
I bought mine at the only dealer in the entire Atlantic Canada region and it's within walking distance of the Northumberland Strait, which is part of the Atlantic Ocean.
I noticed from the Legend site that there are two Quebec dealers near the mouth of the St Lawrence River where the water is salty.
Looks like there is at least one dealer on the West Coast too.
  #49   Report Post  
posted to rec.boats
external usenet poster
 
First recorded activity by BoatBanter: Mar 2014
Posts: 811
Default Galvanic corrosion

On 5/20/2014 8:14 AM, H*a*r*r*o*l*d wrote:
On 5/20/2014 6:57 AM, True North wrote:
Yes Tim, I did tell them my favorite boating destinations...which are
all salt water.
Unless you have cottage on a lake and plan to just leave the boat
there, you'd really be limiting yourself in this area.
All the interesting areas to cruise are on the ocean.

Does your boat builder have a dealership at an ocean location?


Don. Here's a guide to help you select a proper boat
  #50   Report Post  
posted to rec.boats
external usenet poster
 
First recorded activity by BoatBanter: Feb 2014
Posts: 3,524
Default Galvanic corrosion

On 5/20/14, 8:39 AM, True North wrote:
Duh, Jimmy.
I bought mine at the only dealer in the entire Atlantic Canada region and it's within walking distance of the Northumberland Strait, which is part of the Atlantic Ocean.
I noticed from the Legend site that there are two Quebec dealers near the mouth of the St Lawrence River where the water is salty.
Looks like there is at least one dealer on the West Coast too.



If you need yet another reason to put FlaJim in your bozo bin, you have
it. The only reason he posts here is to see if he can aggravate those
who don't share his asshole political opinions. Why toss him a bone he
can chew on by acknowledging his posts? Like several of the righties who
pollute this newsgroup, he is boatless and whatever boating knowledge he
might have had ended when those 1970 and 1980 outdrives gave up the ghost.
Reply
Thread Tools Search this Thread
Search this Thread:

Advanced Search
Display Modes

Posting Rules

Smilies are On
[IMG] code is Off
HTML code is Off
Trackbacks are On
Pingbacks are On
Refbacks are On


Similar Threads
Thread Thread Starter Forum Replies Last Post
Severe galvanic corrosion video Chuck General 18 September 15th 08 02:21 AM
Corrosion - Good Products to Remove Aluminum Corrosion ? B1ackwater General 8 March 31st 06 12:48 AM
Galvanic corrosion and Radio Brian Reay Electronics 5 January 22nd 05 09:21 PM
Seamanship Question #17 Galvanic Corrosion N1EE ASA 9 December 3rd 04 12:28 AM
galvanic corrosion Jean Electronics 2 October 8th 03 02:58 PM


All times are GMT +1. The time now is 09:03 AM.

Powered by vBulletin® Copyright ©2000 - 2025, Jelsoft Enterprises Ltd.
Copyright ©2004-2025 BoatBanter.com.
The comments are property of their posters.
 

About Us

"It's about Boats"

 

Copyright © 2017