On 5/17/2014 6:33 AM, True North wrote:
Yesterday I was on the Legend website where they have a chat function.
I asked the rep about the snaps and she confirmed that they were indeed stainless steel.
She then asked if I had any other concerns.
I felt chatty so I informed her about the corrosion problem... not really expecting to much back.
She went right to the warranty manager and quoted him as saying salt water corrosion was an unpredictable process and not really a warranty problem. He also stated they didn't recommend their boats be used in salt water.
First I heard of this and no where have I seen this in writing nor did the dealer mention it.
They did say to forward pictures of the blisters and they would consult with the dealer on what to do.
Looks like I may be looking for a good Jewish lawyer.

A good Jewish lawyer wouldn't take your case. If you want to prevent
further disintegration of your boat, don't use it in salt water. Do you
know what the third least noble metal next to lead and magnesium is?
Hint. It's one of the materials that Mercury Marine recommends as a
sacrificial anode.
 
Thread Tools Search this Thread
Search this Thread:

Advanced Search
Display Modes

Posting Rules

Smilies are On
[IMG] code is Off
HTML code is Off
Trackbacks are On
Pingbacks are On
Refbacks are On


Similar Threads
Thread Thread Starter Forum Replies Last Post
Severe galvanic corrosion video Chuck General 18 September 15th 08 02:21 AM
Corrosion - Good Products to Remove Aluminum Corrosion ? B1ackwater General 8 March 31st 06 12:48 AM
Galvanic corrosion and Radio Brian Reay Electronics 5 January 22nd 05 09:21 PM
Seamanship Question #17 Galvanic Corrosion N1EE ASA 9 December 3rd 04 12:28 AM
galvanic corrosion Jean Electronics 2 October 8th 03 02:58 PM


All times are GMT +1. The time now is 02:21 AM.

Powered by vBulletin® Copyright ©2000 - 2025, Jelsoft Enterprises Ltd.
Copyright ©2004-2025 BoatBanter.com.
The comments are property of their posters.
 

About Us

"It's about Boats"

 

Copyright © 2017