I use a weak solution of nitric acid to passivate stainless. (I don't
remember, off hand what the mix is. I just keep about 5 gals mixed in a
plastic drum and hang the part in it for a few hours.)

A welder friend has a jelly solution that has nitric acid in it. He brushes
it on a finished stainless weld and lets it set for a couple hours then
rinse it off. Really cleans the weld effected area and never seems to rust
afterwards. Very expensive (about 15 bucks for a half pint jar.)

--
My opinion and experience. FWIW

Steve
s/v Good Intentions


  #2   Report Post  
Doug Dotson
 
Posts: n/a
Default Rust on Stainless Steel

That sounds like WitchNox. It is a bit expensive but it goes a long way.

Doug
s/v Callista

"Steve" wrote in message
...
I use a weak solution of nitric acid to passivate stainless. (I don't
remember, off hand what the mix is. I just keep about 5 gals mixed in a
plastic drum and hang the part in it for a few hours.)

A welder friend has a jelly solution that has nitric acid in it. He

brushes
it on a finished stainless weld and lets it set for a couple hours then
rinse it off. Really cleans the weld effected area and never seems to rust
afterwards. Very expensive (about 15 bucks for a half pint jar.)

--
My opinion and experience. FWIW

Steve
s/v Good Intentions




  #3   Report Post  
OMOO
 
Posts: n/a
Default Rust on Stainless Steel

Citric acid 910%) works as well as nitric and is much safer - see -
http://www.finishing.com/0800-0999/909.html


On Thu, 25 Sep 2003 09:53:52 -0700, "Steve" wrote:

I use a weak solution of nitric acid to passivate stainless. (I don't
remember, off hand what the mix is. I just keep about 5 gals mixed in a
plastic drum and hang the part in it for a few hours.)

A welder friend has a jelly solution that has nitric acid in it. He brushes
it on a finished stainless weld and lets it set for a couple hours then
rinse it off. Really cleans the weld effected area and never seems to rust
afterwards. Very expensive (about 15 bucks for a half pint jar.)



Reply
Thread Tools Search this Thread
Search this Thread:

Advanced Search
Display Modes

Posting Rules

Smilies are On
[IMG] code is Off
HTML code is Off
Trackbacks are On
Pingbacks are On
Refbacks are On


Similar Threads
Thread Thread Starter Forum Replies Last Post
In Search of Stainless Steel Staples Douglas St. Clair Boat Building 7 May 13th 04 05:18 PM
Stainless Steel Boat? CCred68046 General 7 March 25th 04 04:32 AM
Stainless steel running gear kim Boat Building 6 October 22nd 03 01:01 PM
5mm thick stainless steel occ Cruising 0 August 12th 03 03:35 PM
5mm thick stainless steel occ Cruising 0 August 12th 03 03:33 PM


All times are GMT +1. The time now is 03:31 PM.

Powered by vBulletin® Copyright ©2000 - 2025, Jelsoft Enterprises Ltd.
Copyright ©2004-2025 BoatBanter.com.
The comments are property of their posters.
 

About Us

"It's about Boats"

 

Copyright © 2017