Try WichNox by Wichard. Apply with a cloth, let sit for 30 minutes,
then hose off. Alot less effort than NevrDull although NeverDul is good for touchup. BrassO was invented by the military for develop character and combat boredom at sea ![]() Doug "Rick Dunklee" wrote in message ... As "Murphy" says, Stainless Steel isn't"! I have spots of rust on my bow rail from salt water spray. Whats the best way to restore the rail with out marring it? Rick Dunklee "Dawn's Early Light" |
#2
![]() |
|||
|
|||
![]()
toothpaste works too
"Rick Dunklee" wrote in message ... As "Murphy" says, Stainless Steel isn't"! I have spots of rust on my bow rail from salt water spray. Whats the best way to restore the rail with out marring it? Rick Dunklee "Dawn's Early Light" |
#3
![]() |
|||
|
|||
![]()
"On and Off" is what I use. Put it on with a cheap brush and hose it off. You
can buy muriatic acid a lot cheaper - works almost as well... John |
#4
![]() |
|||
|
|||
![]()
ss does not like hcl acid destorys passivation - use ospho or mild rubing
compound - "on-Off will cause future buildup faster - always use high grade wax to protect and clean often - remember it is stainless not no stain steel "Truelove39" wrote in message ... "On and Off" is what I use. Put it on with a cheap brush and hose it off. You can buy muriatic acid a lot cheaper - works almost as well... John |
#5
![]() |
|||
|
|||
![]()
Funny, but my passivated SS (chainplates) don't rust...only handrails, etc.
John ss does not like hcl acid destorys passivation - |
Reply |
|
Thread Tools | Search this Thread |
Display Modes | |
|
|
![]() |
||||
Thread | Forum | |||
In Search of Stainless Steel Staples | Boat Building | |||
Stainless Steel Boat? | General | |||
Stainless steel running gear | Boat Building | |||
5mm thick stainless steel | Cruising | |||
5mm thick stainless steel | Cruising |