Check out WhitchNox. Made by Witchard. Wipe it on with a cloth, let set
for 30 minutes then hose it off. Maybe a quick polishing after to make it really shiney. NevrDull is good for light work. BrassO was invented by the military to build character and to keep sailors minds off of the numming boredom of long seatime ![]() Doug "Rick Dunklee" wrote in message ... As "Murphy" says, Stainless Steel isn't"! I have spots of rust on my bow rail from salt water spray. Whats the best way to restore the rail with out marring it? Rick Dunklee "Dawn's Early Light" |
#2
![]() |
|||
|
|||
![]()
"Doug Dotson" wrote in message ...
Check out WhitchNox. Made by Witchard. Wipe it on with a cloth, let set for 30 minutes then hose it off. Maybe a quick polishing after to make it really shiney. Doug's right, though it's spelled "Wichinox." Contains phosphorus, supposedly. Works for me. E.J. Bleendreeble http://www.casualsailor.com |
#3
![]() |
|||
|
|||
![]()
Is that the stuff that's supposed to passivate the SS?
I've also had good luck with 3M's metal polish and restorer, but I like to use Nevr-Dull first if possible. "EJBleendreeble" wrote in message om... "Doug Dotson" wrote in message ... Check out WhitchNox. Made by Witchard. Wipe it on with a cloth, let set for 30 minutes then hose it off. Maybe a quick polishing after to make it really shiney. Doug's right, though it's spelled "Wichinox." Contains phosphorus, supposedly. Works for me. E.J. Bleendreeble http://www.casualsailor.com |
#4
![]() |
|||
|
|||
![]()
I use a weak solution of nitric acid to passivate stainless. (I don't
remember, off hand what the mix is. I just keep about 5 gals mixed in a plastic drum and hang the part in it for a few hours.) A welder friend has a jelly solution that has nitric acid in it. He brushes it on a finished stainless weld and lets it set for a couple hours then rinse it off. Really cleans the weld effected area and never seems to rust afterwards. Very expensive (about 15 bucks for a half pint jar.) -- My opinion and experience. FWIW Steve s/v Good Intentions |
#5
![]() |
|||
|
|||
![]()
That sounds like WitchNox. It is a bit expensive but it goes a long way.
Doug s/v Callista "Steve" wrote in message ... I use a weak solution of nitric acid to passivate stainless. (I don't remember, off hand what the mix is. I just keep about 5 gals mixed in a plastic drum and hang the part in it for a few hours.) A welder friend has a jelly solution that has nitric acid in it. He brushes it on a finished stainless weld and lets it set for a couple hours then rinse it off. Really cleans the weld effected area and never seems to rust afterwards. Very expensive (about 15 bucks for a half pint jar.) -- My opinion and experience. FWIW Steve s/v Good Intentions |
#6
![]() |
|||
|
|||
![]()
Citric acid 910%) works as well as nitric and is much safer - see -
http://www.finishing.com/0800-0999/909.html On Thu, 25 Sep 2003 09:53:52 -0700, "Steve" wrote: I use a weak solution of nitric acid to passivate stainless. (I don't remember, off hand what the mix is. I just keep about 5 gals mixed in a plastic drum and hang the part in it for a few hours.) A welder friend has a jelly solution that has nitric acid in it. He brushes it on a finished stainless weld and lets it set for a couple hours then rinse it off. Really cleans the weld effected area and never seems to rust afterwards. Very expensive (about 15 bucks for a half pint jar.) |
Reply |
Thread Tools | Search this Thread |
Display Modes | |
|
|
![]() |
||||
Thread | Forum | |||
In Search of Stainless Steel Staples | Boat Building | |||
Stainless Steel Boat? | General | |||
Stainless steel running gear | Boat Building | |||
5mm thick stainless steel | Cruising | |||
5mm thick stainless steel | Cruising |