Oops! Acid flux depends on being washed off after soldering. Might this be
a problem? Roger http://home.insightbb.com/~derbyrm "Glenn Ashmore" wrote in message news:mUiQf.497330$0l5.326643@dukeread06... snip With my small diameter tube I am not to worried about the bond but I will sand blast the whole bolt frame/condenser assembly and paint the tubing with an acid flux formulated for tinning copper pots. I found that the copper/nickel wets out much better with it than regular acid solder flux. |