"brian whatcott" wrote in message
... Bob La Londe wrote: /snip/ I took a good stainless brush and polished the inside of the angled and then welded a bead right down the inside. No worries about air contamination since there is no opening to the other side. No back chipping necessary. Wire-feed? Mig? Tig? Bronze weld stick?? My work pieces and experimental pieces were MIG welded with a big blue 212 is 5000 series wire (I can never remember without looking it up) on 5052 ..125 sheet. |