... Thanks, folks! Yes, my mistake on the location. It's where the sides meet the bottom. If it was higher up, I wouldn't be as concerned. But, it's right where it chages shape in the side to bottom transition, right in the middle along the length, ie. almost under the portage yoke, below the water line for sure. The depressions are only on the outside, and as mentioned, they don't penetrate either the skin or the interior. Spend the extra $100. Sounds odd that OT would let something that obvious out with their name on it. My vote, Fred Klingener |