David Flew wrote:

Aluminum dust is added to aircraft dope to make what we call "silver"
coats. The aluminum dust provides UV protection for the fabric
underneath..

I've done some fiberglass parts that way too.
It works fine.

Richard


I guess the pockets comment means it's expensive ....
David


Probably not outrageously,
but more so that a coat of paint.

Thing is, when the paint ages and deteriorates,
so does the UV protection...

Richard
 
Thread Tools Search this Thread
Search this Thread:

Advanced Search
Display Modes

Posting Rules

Smilies are On
[IMG] code is Off
HTML code is Off
Trackbacks are On
Pingbacks are On
Refbacks are On


Similar Threads
Thread Thread Starter Forum Replies Last Post
Epoxy or Polyester for Fixing Rotten Core on Deck? [email protected] Boat Building 16 January 8th 06 01:18 AM
Epoxy vs. Polyester Terry Spragg Boat Building 0 December 7th 05 01:22 AM
Thinning epoxy barrier coat Robert or Karen Swarts Boat Building 23 December 6th 05 08:36 PM
Epoxy vs. Polyester Matt Colie Boat Building 1 December 6th 05 05:31 PM
Epoxy fibreglass on top of epoxy primer seagoat Boat Building 2 December 1st 05 11:59 AM


All times are GMT +1. The time now is 05:31 AM.

Powered by vBulletin® Copyright ©2000 - 2025, Jelsoft Enterprises Ltd.
Copyright ©2004-2025 BoatBanter.com.
The comments are property of their posters.
 

About Us

"It's about Boats"

 

Copyright © 2017