joe anglim
 
Posts: n/a
Default Chainplate pitting corrosion

I am in the process of refitting a santana 22 that will be used on the
san francisco bay, and will be replacing the standing rigging. The
upper and lower shrouds on each side attach to one chainplate. This
chainplate is located about 18" inboard of the beam, passes through
the cabintop, and is throughbolted to the main bulkhead.

That's all the background, now the problem. I have the chainplates
out, and have found an area of pitting in the stainless (grade
unknown) that is about 1" wide and 2 1/2" tall, with a few small
isolated pits outside of this area. The pits range from barely a
pinhole with almost no depth, to nearly 1/16" diam by nearly 1/16"
deep. All of the pitting is in the area where the plate passes
through the deck, and there is evidence on the bulkhead of water
getting through the deck seal.
The plate is 2" wide, 1/4" thick, and about 18" long. the shrouds
attached are 5/32" upper and 3/16" lower. The boat is about 35 years
old, but the original chainplates from Schock were 1/4" aluminum
plate, and I don't know how far back the stainless plates were put in.

I have gotten three opinions on whether the pitting is a big deal or
not:

1. YES, it's a big deal, the pitting will continue and likely extends
beyond what is visible now. Replace the plates immediately.

2. No, it's insignificant, the plate is way, way, way oversized and a
little pitting won't hurt a bit. You could lift the boat (2600 lbs
unloaded) with a plate half that size.

3. Probably not. Just paint the area of the plate that will be
sealed off from the atmosphere before reinstalling to prevent further
pitting.

The machine shop offering the third opinion also said that they could
fabricate two new chainplates for $200 us.

Relative to the cost of things on this boat, $200 is a large sum and I
don't want to throw it away on servicable parts, but I also don't want
to suffer a dramatic failure out on the bay.

In the realm of peace of mind, my wife / co-owner was present to hear
the first and most troubling opinion, but not the other more calming
opinions.

any thoughts?

thanks,
Joe
 
Thread Tools Search this Thread
Search this Thread:

Advanced Search
Display Modes

Posting Rules

Smilies are On
[IMG] code is Off
HTML code is Off
Trackbacks are On
Pingbacks are On
Refbacks are On


Similar Threads
Thread Thread Starter Forum Replies Last Post
removing corrosion William G. Andersen General 12 June 11th 04 07:25 PM
Parker boat trim corrosion JamesgangNC General 1 June 10th 04 03:22 PM
Corrosion Questions Dave Alonzi General 5 August 8th 03 06:11 PM


All times are GMT +1. The time now is 11:43 AM.

Powered by vBulletin® Copyright ©2000 - 2025, Jelsoft Enterprises Ltd.
Copyright ©2004-2025 BoatBanter.com.
The comments are property of their posters.
 

About Us

"It's about Boats"

 

Copyright © 2017