Reply
 
LinkBack Thread Tools Search this Thread Display Modes
  #1   Report Post  
posted to rec.boats
external usenet poster
 
First recorded activity by BoatBanter: Jul 2008
Posts: 59
Default Severe galvanic corrosion video

http://www.youtube.com/watch?v=IHxFXcGv_Uc

This is bad for an 06 Model!
  #2   Report Post  
posted to rec.boats
HK HK is offline
external usenet poster
 
First recorded activity by BoatBanter: May 2007
Posts: 13,347
Default Severe galvanic corrosion video

Chuck wrote:
http://www.youtube.com/watch?v=IHxFXcGv_Uc

This is bad for an 06 Model!



You have any idea why this is happening?
  #3   Report Post  
posted to rec.boats
external usenet poster
 
First recorded activity by BoatBanter: Mar 2008
Posts: 216
Default Severe galvanic corrosion video

On Sep 11, 12:10*pm, hk wrote:
Chuck wrote:
http://www.youtube.com/watch?v=IHxFXcGv_Uc


This is bad for an 06 Model!


You have any idea why this is happening?


My guess would be shore power
  #4   Report Post  
posted to rec.boats
HK HK is offline
external usenet poster
 
First recorded activity by BoatBanter: May 2007
Posts: 13,347
Default Severe galvanic corrosion video

wrote:
On Sep 11, 12:10 pm, hk wrote:
Chuck wrote:
http://www.youtube.com/watch?v=IHxFXcGv_Uc
This is bad for an 06 Model!

You have any idea why this is happening?


My guess would be shore power



In the absence of anything else, I was going to guess stray currents
(which may well be from shore power) from the boat of a boater in a
nearby slip or dock.

Yet another reason to avoid outdrives! :)
  #5   Report Post  
posted to rec.boats
external usenet poster
 
First recorded activity by BoatBanter: Jul 2008
Posts: 59
Default Severe galvanic corrosion video


"hk" wrote in message
. ..
wrote:
On Sep 11, 12:10 pm, hk wrote:
Chuck wrote:
http://www.youtube.com/watch?v=IHxFXcGv_Uc
This is bad for an 06 Model!
You have any idea why this is happening?


My guess would be shore power



In the absence of anything else, I was going to guess stray currents
(which may well be from shore power) from the boat of a boater in a nearby
slip or dock.

Yet another reason to avoid outdrives! :)


Good guess but not in this case. No shore power, nobody nearby with shore
power, no stray currents etc. Volvo-Penta says they had a bonding or
adhesion problem with the paint they used on some recent outdrives. We are
working with them to get it repainted.



  #6   Report Post  
posted to rec.boats
HK HK is offline
external usenet poster
 
First recorded activity by BoatBanter: May 2007
Posts: 13,347
Default Severe galvanic corrosion video

Chuck wrote:

"hk" wrote in message
. ..
wrote:
On Sep 11, 12:10 pm, hk wrote:
Chuck wrote:
http://www.youtube.com/watch?v=IHxFXcGv_Uc
This is bad for an 06 Model!
You have any idea why this is happening?

My guess would be shore power



In the absence of anything else, I was going to guess stray currents
(which may well be from shore power) from the boat of a boater in a
nearby slip or dock.

Yet another reason to avoid outdrives! :)


Good guess but not in this case. No shore power, nobody nearby with
shore power, no stray currents etc. Volvo-Penta says they had a bonding
or adhesion problem with the paint they used on some recent outdrives.
We are working with them to get it repainted.



Ahhh...boating esoterica...my favorite category! No parts need replacing?

  #7   Report Post  
posted to rec.boats
external usenet poster
 
First recorded activity by BoatBanter: Aug 2008
Posts: 115
Default Severe galvanic corrosion video

On Thu, 11 Sep 2008 23:01:33 GMT, "Chuck" wrote:


"hk" wrote in message
...
wrote:
On Sep 11, 12:10 pm, hk wrote:
Chuck wrote:
http://www.youtube.com/watch?v=IHxFXcGv_Uc
This is bad for an 06 Model!
You have any idea why this is happening?

My guess would be shore power



In the absence of anything else, I was going to guess stray currents
(which may well be from shore power) from the boat of a boater in a nearby
slip or dock.

Yet another reason to avoid outdrives! :)


Good guess but not in this case. No shore power, nobody nearby with shore
power, no stray currents etc. Volvo-Penta says they had a bonding or
adhesion problem with the paint they used on some recent outdrives. We are
working with them to get it repainted.


Were all the anodes in place and properly installed?
  #8   Report Post  
posted to rec.boats
external usenet poster
 
First recorded activity by BoatBanter: Jul 2008
Posts: 8,663
Default Severe galvanic corrosion video

On Thu, 11 Sep 2008 15:57:12 GMT, "Chuck" wrote:

http://www.youtube.com/watch?v=IHxFXcGv_Uc

This is bad for an 06 Model!


That is atrocious.
--
John H.
  #9   Report Post  
posted to rec.boats
external usenet poster
 
First recorded activity by BoatBanter: Jul 2006
Posts: 5,091
Default Severe galvanic corrosion video


"John H." wrote in message
news
On Thu, 11 Sep 2008 15:57:12 GMT, "Chuck" wrote:

http://www.youtube.com/watch?v=IHxFXcGv_Uc

This is bad for an 06 Model!


That is atrocious.
--
John H.



I seem to have a hazy memory of Mercruiser outdrives having a similar
problem for a short period of time.
The cause was the same... the paint used had been changed, either for
"improvement" or, I seem to recall environmental reasons.
Whatever it was, the problem was resolved.

Eisboch


  #10   Report Post  
posted to rec.boats
external usenet poster
 
First recorded activity by BoatBanter: Jul 2008
Posts: 8,663
Default Severe galvanic corrosion video

On Thu, 11 Sep 2008 19:21:54 -0400, "Eisboch" wrote:


"John H." wrote in message
news
On Thu, 11 Sep 2008 15:57:12 GMT, "Chuck" wrote:

http://www.youtube.com/watch?v=IHxFXcGv_Uc

This is bad for an 06 Model!


That is atrocious.
--
John H.



I seem to have a hazy memory of Mercruiser outdrives having a similar
problem for a short period of time.
The cause was the same... the paint used had been changed, either for
"improvement" or, I seem to recall environmental reasons.
Whatever it was, the problem was resolved.

Eisboch


Before my time. I had no problems with my outdrive, but I didn't keep my
boat in a slip either.

I like having the boat on a trailer, in my driveway!
--
John H.
Reply
Thread Tools Search this Thread
Search this Thread:

Advanced Search
Display Modes

Posting Rules

Smilies are On
[IMG] code is Off
HTML code is Off
Trackbacks are On
Pingbacks are On
Refbacks are On


Similar Threads
Thread Thread Starter Forum Replies Last Post
Corrosion - Good Products to Remove Aluminum Corrosion ? B1ackwater General 8 March 31st 06 12:48 AM
Galvanic corrosion and Radio Brian Reay Electronics 5 January 22nd 05 09:21 PM
Seamanship Question #17 Galvanic Corrosion N1EE ASA 9 December 3rd 04 12:28 AM
What to do in a severe knockdown? tom ASA 62 November 5th 04 12:44 PM
galvanic corrosion Jean Electronics 2 October 8th 03 02:58 PM


All times are GMT +1. The time now is 12:53 AM.

Powered by vBulletin® Copyright ©2000 - 2025, Jelsoft Enterprises Ltd.
Copyright ©2004-2025 BoatBanter.com.
The comments are property of their posters.
 

About Us

"It's about Boats"

 

Copyright © 2017