True North wrote:
Went to a local maker of boat covers within walking distance of home and wasn't surprised to hear that they do come across the problem regularly....especially with older boats in for a new cover.
Guh gave me a few tips of how he frees up corroded screws etc.
Then went to the local marine supply store where I talked to an ex coast guard guy who used to install aluminum towers and stainless fittings on our salty coast.
He told me they used nylon washers and gaskets to separate the metals and recommend dedicated a product called Lanocote to apply to the screw shafts.
They didn't carry PB Blaster but he advised that a local hardware store did, so that was my next stop.
Took a peek at their manual impact screw driver, but at $43. I'll see if I really need it.
If I can't find the proper washers locally I may go over time Princess Auto and buy the property sized punch to make my own washers out of ice cream plastic containers.



Now *that's* funny!
 
Thread Tools Search this Thread
Search this Thread:

Advanced Search
Display Modes

Posting Rules

Smilies are On
[IMG] code is Off
HTML code is Off
Trackbacks are On
Pingbacks are On
Refbacks are On


Similar Threads
Thread Thread Starter Forum Replies Last Post
Severe galvanic corrosion video Chuck General 18 September 15th 08 01:21 AM
Corrosion - Good Products to Remove Aluminum Corrosion ? B1ackwater General 8 March 30th 06 11:48 PM
Galvanic corrosion and Radio Brian Reay Electronics 5 January 22nd 05 08:21 PM
Seamanship Question #17 Galvanic Corrosion N1EE ASA 9 December 2nd 04 11:28 PM
galvanic corrosion Jean Electronics 2 October 8th 03 01:58 PM


All times are GMT +1. The time now is 10:48 AM.

Powered by vBulletin® Copyright ©2000 - 2025, Jelsoft Enterprises Ltd.
Copyright ©2004-2025 BoatBanter.com.
The comments are property of their posters.
 

About Us

"It's about Boats"

 

Copyright © 2017