engsol wrote:
...tupperware container... epoxy... Now I have a 6" thru-hull pad which is flat for the nut, and still conforms perfectly to the hull shape. Sounds like a great job. The only refiniement I'd think about is to have put some fiberglass cloth into it, as well as #404 filler. I've had some bad luck with epoxy melting the plastic, trying similar fixes, but am not sure if it was due to chemistry or temp. A bit more clean-up, but no difference in the final result. So, when are you going to come over and do that job on my boat? ![]() Fresh BReezes- Doug King |