steen wrote:
On Sun, 23 May 2004 22:49:19 UTC, "John R Weiss" wrote: the satins are rated for interior use only. Maybe they aren't designed to hold up under hard use, weather, or UV. This is the case. Thanks! You can easily achieve a satin finish with gloss varnish by rubbing it out with fine Scotchbrite, steel wool or bronze wool. It's actually a bit nicer than using satin varnish, since you don't have the flatting agent hiding the wood grain. |