Howdy Evan:

As with all epoxies, the pot life varies dramatically with
temperature... But, during a nice 80 degree day, it's about 50- 60
minutes. I chose this combination due to the fairly low mixed
viscosity of about 450 cps, which gives a nice wet-out to all of the
glass / kevlar I've used to date. Note that the elongation % of
concern is that of the 'system', as opposed to just the hardner. See
for example:

http://69.239.32.181/Jeffco/Systems/...y=1314with3138

which is Jeffco's 1314 resin with the same 3138 hardner. The
elongation of the 'system' with a moderate post-cure is 5.5%, which
compares most favorably to Gougeon's Pro-Set 125/229 at 4.5%.

There used to be a similar 'system' page for the 1310-L6 / 3138
combination, but it looks like they've moved on.

MW

 
Thread Tools Search this Thread
Search this Thread:

Advanced Search
Display Modes

Posting Rules

Smilies are On
[IMG] code is Off
HTML code is Off
Trackbacks are On
Pingbacks are On
Refbacks are On


Similar Threads
Thread Thread Starter Forum Replies Last Post
recommended vendor for 15+ gal epoxy ? Courtney Thomas Boat Building 1 October 24th 05 01:15 AM
nu2 woodworking - my epoxied wood is delaminating,.. James Johnson Boat Building 1 October 23rd 05 05:06 PM
Anybody tried glueing cast aluminum parts together with epoxy? [email protected] Boat Building 23 October 16th 05 07:35 PM
safe breathing apparatus for lead, epoxy, etc. ? Courtney Thomas Cruising 6 October 10th 05 03:16 AM


All times are GMT +1. The time now is 08:07 PM.

Powered by vBulletin® Copyright ©2000 - 2024, Jelsoft Enterprises Ltd.
Copyright ©2004-2024 BoatBanter.com.
The comments are property of their posters.
 

About Us

"It's about Boats"

 

Copyright © 2017