As an aside, be sure to wipe down any fresh glass with acetone prior to
sanding. That removes the blush and insures that overcoats will adhere.

A good source of information about glass and what to put over it can be
found in the publications from the West System people. Many of their
publications are free.

Max


Thanks I'll be sure to do that. The resin I'm using is low blushing
but you can never be too safe in these things.



 
Thread Tools Search this Thread
Search this Thread:

Advanced Search
Display Modes

Posting Rules

Smilies are On
[IMG] code is Off
HTML code is Off
Trackbacks are On
Pingbacks are On
Refbacks are On


Similar Threads
Thread Thread Starter Forum Replies Last Post
Cetol vs Bristol Finish ... NE Sailboat Cruising 27 March 14th 07 01:47 AM
Help with part number wingspan General 3 August 23rd 06 03:42 AM
A Commodores Meanderings: Part 2 RGrew176 General 0 August 3rd 04 03:03 AM
Siphons, anti-siphons & wet exhausts JAXAshby ASA 57 June 19th 04 08:25 PM
RDF for newbies and NN of KN JAXAshby ASA 22 March 11th 04 11:54 PM


All times are GMT +1. The time now is 10:26 AM.

Powered by vBulletin® Copyright ©2000 - 2025, Jelsoft Enterprises Ltd.
Copyright ©2004-2025 BoatBanter.com.
The comments are property of their posters.
 

About Us

"It's about Boats"

 

Copyright © 2017