Default Questions on UV curing polyester resins.

On Tue, 16 Mar 2010 01:35:54 -0700 (PDT), wrote:

On Mar 14, 12:31*pm, Paul Oman wrote:
wrote:
Two questions for people with knowledge or experience with the UV
curing polyester resins:


1) Are they (any of them) compatible with polystyrene foam?


*2) Once the UV light has initiated the polymerization, will it spread
* * * through the layup even into places where the light did not
* * * penetrate? *I'm thinking, for instance about the underside
* * * of carbon fiber cloth.


*Thanks.


--


FF


it makes more sense to use thermo set epoxies. Stronger, better bond,
probably cheaper.
epoxies will not dissolve foam


Thermo set meaning that they don't begin to cure until they are
heated?
I ask because I am looking for a very long working time.

If so, do you have a recommendation?

Otherwise, can you answer the first question? I was quite aware of
the
other issues.



I believe that any of the polymer based resins will destroy
polystyrene foam. At least that was what I was told years ago, but I
must admit that I never tested it.

By the way, UV curing polyester is not essentially a different resin.
It is polyester resin with a UV catalyst added to it and it is the
resin that attacks the foam.

I'm not a board builder but I believe that the polyester boards are
made using polyurethane foam.

Have a look at
http://www.compositesworld.com/artic...s-demonstrated

for more details of using UV polyester

It apparently is possible to laminate carbon fiber with some cautions.

What are you building?

Cheers,

Bruce