"RichH" wrote in message
...
Nylon should be avoided at all cost for applications that are wetted
with water !!!!!!!!
Nylon quickly hydrolyzes (rapid breaking down of the long chain
macromolecules ... analagous to rust (intergrannular corrosion) in
metals); and, rapidly loses material strength. Nylon6 (most common)
is the absolute worst and Nylon66 is close. In industry, the
hydrolysis is usually found after a few months in water wetted
application.

Marelon, etc. is at least stabilized by inhibiters, etc. to better
withstand this hydrolysis.


OY!!

So, I can't find Marelon, can't find Bronze, in the particular
fitting.

Which is better - Nylon or Brass? Perhaps that's the reason for the
failure of the original nylon fitting...

And, by implication ("at least" - "to better withstand"), Marelon
should not be used in any wet applications either??

--
L8R

Skip

Morgan 461 #2
SV Flying Pig KI4MPC
See our galleries at www.justpickone.org/skip/gallery !
Follow us at http://groups.yahoo.com/group/TheFlyingPigLog
and/or http://groups.google.com/group/flyingpiglog

"You are never given a wish without also being given the power to
make it come true. You may have to work for it however."
(and)
"There is no such thing as a problem without a gift for you in its
hands. You seek problems because you need their gifts."
(Richard Bach, in The Reluctant Messiah)