Electrolysis
"Jere Lull" wrote in message
news:2007101318225116807-jerelull@maccom...
On 2007-10-13 11:15:53 -0400, "claus" said:
"Richard Casady" wrote in message
...
On Fri, 12 Oct 2007 19:44:01 -0700, "claus"
wrote:
However, in spite of our best efforts - the prop eventually failed.
Because of our bad experience we decided to replace the folding bronze
prop with a Volvo aluminum prop.
So you feel that a aluminum prop will be less subject to corrosion than
bronze?
Casady
Yes - and it is also less costly to replace ($200. vs $2,500). On the
other hand, I will lose some speed under sail but since I don't race I
can live with that :-)
The aluminum prop will disappear more quickly, sad to say.
Well, in that case the Volvo sail drive housing - mado of aluminum - should
have disappeared long ago - however it is like new after some 5 years....
Also, considering that savings by not having a diver replace the 3 small
zincs on the Volvo bronze folding prop (appproximately 4 times a year x
$100.) it is still less costly to replace the aluminum prop say once a year
if needed.
|