Talking about how to revive cloudy/crystallized resin and clean pumps. I
guessed 180 degrees F. The correct value is 120 degrees F.
Sorry.
Roger (like I said, I just eyeballed the goop and stopped when it got clear
and shiny)
http://home.insightbb.com/~derbyrm
P.S. Tower Hobbies has a neat non-contact temperature gauge for under $30
delivered.