I don't know how big the piece is. When laying up CF I wet out as
described and then use a hard roller and paper towel to remove as much
resin as I can before bagging the part. The PT and hard roller between
layers helps get the cloth to resin ratio pretty high.


On Fri, 26 Aug 2005 05:57:38 +1000, "AD"
wrote:

Thanks Jim,

Thats pretty much what I do too. I tend to be a bit heavier on the resin,
particularly on the heavier carbon double bias cloth and then remove the
excess by bagging, just to be sure.

regards,

AD