Default Epoxy fairing compound and glassing hull


"Glenn Ashmore" wrote in message

I used the Tom Sawyer approach and got a bunch of volunteers. One
person mixing resin, two people wetting out and 3 people laying. We did
two layers of DB170 biax and one 6 oz. woven on my 45' hull in 6 hours.
After wetting out on a table made from a couple of sheets of melamine
we rolled the biax on 2" PVC pipe to carry it to the boat. The only
significant increase in cost was a couple of cases of beer when we
finished.


Glenn,

Did you ever get your home made fabric impregnator to work?

About how many yards / square meter of fabric did each 6 hour session manage
to lay up?

And how much experience did your wetting out team have?

Thanks

--